There are 3 objects for which Condition contains → unglazed
13.10.27 Intact, small piece missing from one side of the wick rest. White deposit in places, blackening around the wick rest, probably from use. Unglazed.
78.12.18 Intact, a few chips around outside of rim, scratches on inside and underside. Base roughened. Small amount of black at the end of the wick rest, white deposit in places. Two small holes, one on the underside of the rim, the other on the base. Unglazed.
78.12.3 Intact, slight chipping around the nozzle obscuring one of the volutes, the other is very faded as is the moulded design. very small amount of grey deposit. Unglazed.